Street Rodder Magazine Homepage

Applying Lead Body Work

Matt hand-sanded the welding spatter on the open surfaces with 80-grit paper and followed up final prep with 180-grit on any smooth areas to promote plenty of adhesion. It's critical to have the surface properly prepared before proceeding any further.
How to Apply Lead - Get The Lead Out

Matt hand-sanded the welding spatter on the open surfaces with 80-grit paper and followed up final prep with 180-grit on any smooth areas to promote plenty of adhesion. It's critical to have the surface properly prepared before proceeding any further.  View Related Article

 