Fabricating Stainless Steel Doorsills
|
I then swapped the rear and front brake fingers from right to left to form the shorter forward portion of the sill, which flares out wider toward the front of the sill. As the angle of the radius changes, the sheetmetal was once again heated while being slowly bent, which allowed the metal to shrink at the inside angle. View Related Article
|
|